How to Choose Gate Location and Gate Type for Injection Molded Parts

Cross-section illustration of an injection mold showing melt entering a cavity through an edge gate, with the gate, runner and part labelled

A buyer looks at a first sample and sees a faint line across the middle of the cover, a small scar on the one face that had to stay clean, and a dip over the screw boss. Three different problems, one common cause: the gate was put in the wrong place, or the wrong type of gate was chosen for the part.

Choose the gate for the part, not for the mold: put the gate where the melt can flow from the thickest section toward the thinnest, keep its mark off every cosmetic face, and pick the gate type whose vestige — the small mark left after the runner is removed — your part can carry. Agree the gate type, its position, and the vestige limit in writing before steel is cut, because moving a gate after tooling means cutting new steel.

This guide explains what a gate is, compares the gate types a mold maker is likely to propose, gives the placement rules that prevent the common failures, and ends with a checklist you can put in the RFQ.

What a gate is, and what it decides

A gate is the small opening in the mold through which molten plastic enters the cavity. It is the last part of the feed system: melt travels from the machine nozzle through the sprue and the runner, then through the gate into the cavity. Once the part is ejected, the sprue, runner, and the small piece of plastic in the gate are trimmed away — by hand, by fixture, or automatically as the mold opens. What remains on the part is the gate vestige, sometimes called a witness mark.

That small opening decides more than most buyers expect:

  • How the part fills. The gate sets where the flow starts, so it sets the flow direction, the flow length to the farthest corner, and where two flow fronts meet and form a weld line.
  • How the part packs. Packing pressure can only reach the part while the gate is still open. A gate that freezes early cuts off packing, and the thick sections behind it shrink without compensation — which is how sink marks appear over ribs and bosses.
  • What the surface looks like. Every gate leaves a mark. Its size and position are fixed by the gate type and location, and no amount of polishing after molding removes a gate scar from a cosmetic face.
  • How much the part costs. A gate that degates automatically saves trimming labor on every part. A gate that needs hand trimming adds a manual step to every cycle. A hot-runner gate removes the cold runner entirely, but the mold costs more.

Protolabs puts the practical rule simply in its gating guide: gates can and should be placed in non-cosmetic areas whenever possible, and where a gate must sit in a less-than-ideal area, steps can be taken to minimize the mark. The rest of this guide is how to make those two decisions — type and position — deliberately, instead of discovering them at the first trial.

The gate types, compared

A mold maker will usually propose one of the families below. The table reads left to right: where the gate feeds, what mark it leaves, what it suits, and what to watch for.

Gate typeWhere it feedsVestige left on the partBest forWatch out for
Edge gateAt the parting line, into the edge of the partA rectangular scar along the edge, typically trimmed by hand or fixtureThe default for flat or boxy parts; the easiest gate to enlarge or move in steelThe scar sits on the edge; not suitable where the edge is a sealing or visible face
Tab gateAt the parting line, through a small tab attached to the partThe scar is on the tab, which is removed — the part face stays cleanCosmetic parts where the gate must not touch the part itselfExtra trimming step; the tab adds a small amount of material and handling
Fan / film gateA wide, shallow edge gate spread across a broad frontA wide linear trim line along the edgeFlat panels, covers, and thin-walled parts that must fill evenly with little warpageWider trim area; needs a fixture or router to remove cleanly
Submarine (tunnel) gateAn angled tunnel below the parting line, into a rib or non-cosmetic wallA small oval shear mark where the tunnel breaks offAutomatic degating in higher volumes; no hand trimmingThe tunnel is small, so it suits smaller parts; brittle or highly glass-filled resins can chip or leave shear dust when the gate breaks
Cashew (banana) gateA curved tunnel below the parting line, reaching an inside surfaceA small mark on an inside face, sheared off automaticallyParts that must be gated from the moving side, where no edge is availableComplex to machine and to maintain; placement is tightly constrained
Pin point gateA small hole through a three-plate mold, onto the top face of the partA small raised or recessed point on the faceCenter gating of round or deep parts; balanced fill from the middle outwardNeeds a three-plate mold, which adds cost and press daylight; the cold runner still has to be reground or discarded
Diaphragm gateA disc of plastic across the whole opening of a round partA trim line around the full openingRound parts with large open diameters — caps, bezels, rings — where even filling matters and weld lines must be avoidedThe whole diaphragm must be trimmed away; only fits parts with a suitable opening
Ring gateA ring around a core pin, feeding a tube or round part from all sidesA trim line around the circumferenceTubes and cylindrical parts that must stay concentricTrimming all around the part adds a step
Direct sprue gateDirectly from the sprue into the broadest section of the partA large circular mark, usually needing machining or fixture trimming to removeSingle-cavity parts, very large parts, or high glass-fill resins that need a large gateThe largest vestige of any gate; only for single-cavity tools
Hot tip gateA heated nozzle tip delivers melt directly to the cavity wall, with no cold runnerA small conical nib or dimple, often hidden in a recess or logoCosmetic parts and multi-cavity tools where runner waste must go; good for centre gatingCan leave blush or circular flow marks around the gate, which is a problem on a cosmetic face; small gates can plug with high glass-fill resins
Valve gateA heated nozzle with a mechanical pin that shuts the gate flush with the cavity wallA clean, flat circular witness ring, close to zero raised materialThe cleanest cosmetic result and the best control of packing; sequential valve gates can move weld lines deliberatelyThe highest tooling cost of any gate here, plus controller and maintenance

Two points in that table deserve emphasis, because they are the ones buyers most often get wrong.

First, the cheapest gate is not the cheapest part. An edge gate costs the least in steel, but every part then carries a hand-trimming step. At 100,000 parts a year, a submarine or valve gate that degates automatically can be cheaper than a "cheap" edge gate, even though the mold costs more. Ask the mold maker to price both the tool and the per-part degating step before you choose.

Second, hot-runner gates are a system, not a gate type. A hot tip or valve gate needs a heated manifold, a controller, and maintenance. Our guide to hot runner injection molding explains the trade-offs in full — the summary is that hot runners remove runner waste and shorten cycle time, but they raise the mold cost and need a maintenance plan. Do not accept a hot-runner gate on a low-volume part without seeing the cost comparison.

For an independent description of the same gate families, see Xometry’s types of injection molded gates and Protolabs’ solving gating problems in injection molding.

Where to put the gate: seven placement rules

Gate type is half the decision. Position is the other half, and it is the half that causes most first-trial failures. Use these rules in order; when two rules conflict, the earlier one usually wins, and the conflict itself should be recorded in the design review.

1. Gate into the thickest section, and let the flow run from thick to thin. Melt should enter where the wall is thickest and flow toward the thinner areas. A gate in a thin wall freezes before the thick section behind it is packed, and the thick section then sinks. If the part has a boss or a heavy section, the gate should feed that section — or as close to it as the part allows.

2. Keep the gate and its vestige off every cosmetic face. Mark the cosmetic faces — the A-side surfaces the customer sees — on the drawing before the gate is proposed. The gate belongs on a hidden face, an edge, or inside a recess. If no hidden face exists, choose a gate whose vestige can be hidden in a logo, a texture change, or a recess, and agree the vestige limit in writing. A gate scar on a polished face is not a process problem; it is a design decision that was never made.

3. Aim the flow at a wall, never into open space. Melt shooting from a gate straight into an empty cavity forms a snaking jet, which leaves flow marks and trapped air. The gate should direct the melt against a wall or a core pin so the flow front spreads evenly. This is one reason edge gates are placed at the parting line: the melt meets the wall immediately.

4. Put the gate where the weld line can be tolerated. Wherever the flow splits around a hole, a boss, or a core pin, the two fronts meet again and form a weld line — a visible seam and a weaker section. Gate position decides where that line falls. It should fall on a non-cosmetic area, away from any feature that carries load, and never across a screw boss or a snap-fit root. If the weld line cannot be moved to a safe place, consider a second gate, a different gate type, or a flow simulation before steel is cut.

5. Balance the flow in multi-cavity molds. In a multi-cavity tool, every cavity must fill at the same time and pack to the same weight. Gates that differ in size or distance from the sprue will fill unevenly, and one cavity will flash while another short-shots. The runner layout and the gate sizes must be balanced together; a balanced runner with unbalanced gates is still unbalanced.

6. Gate close enough to pack, far enough to cool. Packing pressure only works while the gate is open, so the gate must be large enough — and the wall at the gate thick enough — to stay open until the part is packed. A gate that is too small freezes early and the part sinks; a gate that is too large leaves a big vestige and a long freeze time that stretches the cycle. Published gate-design guides commonly use an edge-gate depth of about 50–75% of the nominal wall as a starting point, with the final size confirmed by the mold maker for the resin, the wall thickness, and the part weight. Ask for the gate size and the gate-freeze time to be recorded at the first trial, so the packing window is evidence, not a guess.

7. Check the gate against ejection, cooling, and venting. A gate next to an ejector pin can leave a sink mark on the opposite face. A gate far from the cooling circuits can leave a hot spot that warps the part. And the last place the melt reaches — the end of fill — needs a vent, or trapped air will burn or block the fill. Gate position, cooling, and venting are one design problem, not three separate ones.

When the rules conflict, say so in the review. A common conflict is rule 1 against rule 2: the thickest section is on the cosmetic face. The honest answers are a tab gate that moves the scar onto a removable tab, a submarine gate that feeds from below the parting line, or a valve gate hidden in a recess. What is not an answer is to gate the thin cosmetic wall and hope the process compensates.

A worked example: choosing a gate for a housing cover

The example below is illustrative, with stated assumptions — it is not a quotation, and the right gate for a real part depends on the drawing, the resin, and the mold maker’s review.

Take a rectangular housing cover, 150 mm long, 100 mm wide, 25 mm deep, with a 2.5 mm nominal wall, two screw bosses on the inside, and a polished outer face that the customer sees. The resin is ABS. The annual volume is 50,000 parts.

Three gate proposals are on the table:

  • An edge gate on the short side, at the parting line. The melt flows along the 150 mm length, from the thick edge toward the far wall. The weld line forms at the far end, away from the bosses. The vestige is a rectangular scar on the short edge, which is hidden when the cover is assembled. Degating is manual. This is the simplest proposal, and the one most mold makers would offer first.
  • A hot tip gate in the centre of the polished outer face. The melt flows radially outward, so the fill is balanced and the bosses pack well. But the gate sits on the one face that must stay clean, and a hot tip can leave blush — a circular flow mark — around the gate. Hiding the nib in a logo recess helps, but the blush risk stays. The mold costs more, and the runner waste disappears.
  • A submarine gate into the inside rib, below the parting line. The melt enters through a tunnel and the gate shears off automatically when the mold opens, so there is no hand trimming. The vestige is a small oval mark on the inside rib, invisible in use. But the tunnel is small, and the flow must travel farther to reach the far wall, so the packing window is tighter and the gate-freeze time must be checked at the first trial.

The decision turns on the cosmetic requirement. If the polished outer face must stay perfect, the hot tip gate is out — its blush risk is on exactly the wrong face. Between the edge gate and the submarine gate, the trade is manual trimming on every part against a tighter packing window and a more complex mold. At 50,000 parts a year, the automatic degating of the submarine gate is worth the extra mold complexity, provided the first trial confirms the gate stays open long enough to pack the bosses. If the trial shows sink over the bosses, the answer is a larger gate or a second gate, not more packing pressure — pressure cannot pass a frozen gate.

The point of the example is not which gate wins. It is that the choice is made by weighing fill, vestige, and degating cost against each other, on the actual part, before steel is cut. A gate review that only asks "where is the gate?" is not a review. It should ask: where does the flow go, where does the weld line land, what does the vestige look like, and who trims it?

What goes wrong when the gate is wrong

Most gate problems show up at the first trial, and each one points back to a specific gate decision:

Symptom at T1Likely gate causeFirst check
Jetting — snaking flow marks from the gateMelt entering an open cavity instead of hitting a wallGate direction and position; aim the flow at a wall or core pin
Weld line across a loaded feature or a cosmetic faceFlow splitting around a hole or boss and meeting in the wrong placeGate position; move the gate or add a second gate so the weld line falls somewhere safe
Sink mark over a boss or thick sectionGate froze before the thick section was packedGate size and gate-freeze time; part weight as packing time changes
Blush or circular flow marks around the gateHot tip gate on a cosmetic face, or gate too small for the resinGate type; consider a tab or edge gate, or hide the gate in a recess
Flash at the gate or parting lineGate too large, or packing pressure held after the gate should have frozenGate size, packing profile, and clamp force
Short shot at the far end of the partGate too small, too far from the thick section, or frozen earlyGate size and position; flow length from gate to last-fill area
Visible gate scar on a cosmetic faceGate type or position chosen without marking the cosmetic facesThe drawing: mark A-side faces and the vestige limit before the next tool
One cavity flashes while another short-shotsUnbalanced gates or runners in a multi-cavity toolGate sizes and runner balance, cavity by cavity

If a symptom appears on only one cavity, the cause is almost certainly in that cavity’s gate or runner, not in the process settings. Do not tune the machine to fix a single-cavity problem.

Gate checklist for the RFQ and the drawing

Put these items in the RFQ package, and check them off before the mold design is approved:

  • Cosmetic (A-side) faces marked on the drawing, with the surface finish for each
  • Gate type proposed by the mold maker, with the reason it was chosen over the alternatives
  • Gate position marked on the mold design, and the flow direction it creates
  • Expected weld-line positions marked, and confirmed away from loaded features and cosmetic faces
  • Gate vestige limit stated — maximum height and location — and how it will be trimmed
  • Degating method stated: manual, fixture, or automatic, and who pays for the step
  • Gate size stated, with the wall thickness at the gate and the resin grade it was sized for
  • Hot runner or cold runner stated; if hot runner, the nozzle type, controller, and maintenance plan
  • Gate-freeze time and part-weight record required at T1, so packing is proven, not assumed
  • First-article photos of the gate area, the weld-line area, and the cosmetic faces required with the T1 report
  • Cost of moving a gate after tooling started stated, or capped in writing

Our T1 sample approval guide explains what evidence to require before production is released, and our guide to choosing wall thickness explains why uniform walls make the gate’s job possible in the first place. Gate position also decides whether a living hinge survives — our living-hinge guide shows why the melt must flow across the hinge, not along it.

Frequently asked questions

Can the gate be moved after the mold is built?

Sometimes, but it is a steel change, not a setting change. Moving a gate means welding and re-cutting the gate area, re-balancing the runner, and re-running the trial — and the old gate location leaves a mark on the mold that may still show on the part. It is far cheaper to agree the gate position during the mold design review than to move it after the first trial. Ask what a gate move costs before you approve the design, so the number is known in advance.

Is a valve gate always the best choice for cosmetic parts?

No. A valve gate gives the cleanest vestige and the best packing control, but it is also the most expensive gate in the table and it needs a hot-runner system, a controller, and maintenance. For many cosmetic parts, a tab gate or a submarine gate gives an acceptable vestige at a much lower tooling cost. Choose the cheapest gate whose vestige your part can carry, not the most expensive gate available.

How many gates does my part need?

One gate is the default, and it should stay the default unless there is a reason to add another. Add a gate when one gate cannot fill the part without an excessive flow length, when a single weld line cannot be kept out of a loaded area, or when the part is so large that one gate leaves the far end unpacked. Every extra gate adds a weld line where its flow meets the next gate’s flow, so more gates are not automatically better — they are a trade, and the flow simulation or the trial should show the trade before steel is cut.

Agree the gate before the steel is cut

A gate is a small opening with a long memory. Its type decides the mark on the part and the cost of removing it; its position decides the fill pattern, the weld line, and whether the thick sections pack. Both are fixed in the mold design, and both are expensive to change after tooling.

Send the mold maker a drawing with the cosmetic faces marked, the thick sections identified, and the vestige limit stated — and ask for the gate proposal in writing, with the reason, before the design is approved.

If you are ready to discuss a part, send your STEP file, 2D drawing, material, quantities, key tolerances, surface finish, delivery region, and timing through our contact page. Mark the cosmetic faces and any gate restrictions on the drawing, and the gate decision can be made in the design review instead of at the first trial.

Hey! I’m Jerry — a hands-on mold & CNC guy who’s spent years turning ideas into real, tangible products. From tight-tolerance molds to complex machining projects, I’ve seen (and solved) a bit of everything.

Beyond the tools and machines, I’m all about people: building trust, making things easier for clients, and finding smart solutions that work. I’ve worked with teams around the world, and I’m always excited to meet others who love creating and building as much as I do.

If you’re into manufacturing, product development, or just like a good behind-the-scenes look at how things get made — let’s connect!

Send Us Your Requirements

Let's review your mold project

Tell us what you’re building and we’ll help identify the right tooling path. Send your 2D drawing, 3D CAD file, resin, annual volume, tolerances, or target timeline when available.

Engineering-led reviewReply within one business dayConfidential project details

No obligation. We’ll review the information and reply with a practical next step. Prefer email? jerry@cavitymold.com.